| 1.
| Mark out area of contact and clean vehicle paint down to primer surface using 80 grit paper.
|
| 2.
| Prepare contact surface of fibreglass with 80 grit paper.
|
| 3.
| Dry fit panels to check alignment.
|
| 4.
| Wip with moist cloth of cellulose thinners or acetone both contact surfaces proir to application of bond agent.
|
| 5.
| Mix bond agent and apply sufficient amount to both surfaces.
|
| 6.
| Apply pressure and secure panels, removing any excess bonding agent.
|
| 7.
| When fully cured, smooth in joins with polyester body filler ensuring joins are covered.
|
| 8.
| Shape vehicles with 80 grit paper to start and finish off with 240 grit.
|
| 9.
| Vehicle now ready for paint process (see painting advice).
|
|  
|
|  
|
|  
|
|  
|
|  
|